ML-820-S2BYL made in JAPAN Discontinued
- Pitch 7.5mm
 - Stranded wire and Solid wire
 - Check hole
 - Press fit
 
Order model number
- Order model numberML-820-S2BYL-[Position]
 - Order exampleML-820-S2BYL-2P (An example of ordering with 2 positions.)
 
Flow process solder heat resistance
| Pre Heat Temperature | 100-140℃ | 
|---|---|
| Pre Heat Times | 40 seconds | 
| Solder Immersion Temperature | 265±3℃ | 
| Soldering Times | 10±1 seconds | 
Using a Soldering Iron
| Tip Temperature | 390±10℃ | 
|---|---|
| Tip Contact Times | 5±1 seconds | 
| Number of Times | 2 | 
Note
- ・Reflow process is not applicable.
 - ・Perform the second soldering with a soldering iron after the product has cooled sufficiently and returned to room temperature after the first soldering.